What is the most common reason for insufficient material injection into the mold cavity?

1. Poor material fluidity

Material fluidity is one of the key factors affecting the filling effect. When the flowability of plastic is poor, the material flow is difficult to fill the entire cavity, resulting in insufficient filling. This is usually related to the viscosity, temperature, molecular weight distribution of the plastic, as well as the type and content of additives. To improve fluidity, plastics with good fluidity can be selected, or fluidity can be increased by adjusting the plastic formula, such as adding plasticizers, lubricants, etc.

2. Poor exhaust of the mold

Poor exhaust of molds is also an important reason for insufficient filling. During the injection molding process, a large amount of gas is generated when the plastic melt flows in the mold cavity. If the exhaust system design of the mold is unreasonable or the exhaust holes are blocked, these gases cannot be discharged smoothly, forming a high-pressure zone at the end of the mold cavity and hindering further filling of the material flow. To solve this problem, exhaust slots or holes can be opened at appropriate positions in the mold to ensure smooth gas discharge.

3. Front cooling of material flow

During the injection molding process, the material flow front will rapidly cool down upon contact with the mold cooling system, forming a layer of cold material. This layer of cold material will block the gate, runner, and injection port, causing subsequent material flow to be unable to enter the mold cavity smoothly, resulting in insufficient filling. To solve this problem, the size of the cold material well can be expanded to accommodate more cold material and prevent it from blocking the gate and runner.

4. Inconsistent R values between nozzle and mold mouth

The inconsistency between the R values of the nozzle and the die can cause additional resistance to the melt during the spraying process, thereby reducing the effective amount and pressure of the melt and resulting in insufficient filling. To solve this problem, it is necessary to ensure that the R values of the nozzle and the mold are consistent to reduce the resistance of the melt during the spraying process.

5. Excessive feeding amount

Although insufficient feeding can lead to insufficient filling, excessive feeding can also cause problems. When the feeding amount is too large, the effective pressure of the melt will decrease because too much melt will generate additional resistance during the injection process. To solve this problem, it is necessary to reduce the feeding amount and use methods such as feeding throttle plugs to control the excessive feeding of lubricant particles.

6. The nozzle temperature is too low

A nozzle temperature that is too low can cause the temperature of the melt to rapidly decrease during the spraying process, thereby reducing the fluidity of the melt and resulting in insufficient filling. To solve this problem, it is necessary to separate the nozzle from the mold during mold opening to reduce the influence of mold temperature on the nozzle. At the same time, it is necessary to ensure that the nozzle temperature remains within the range specified by the process.

7. Unbalanced pouring system

In a multi cavity mold, if the design of the pouring system is unbalanced, it will cause the cavity far away from the main runner to be unable to be filled. To solve this problem, the pouring system can be balanced by adjusting the gate width size or making the lengths of each part of the runner consistent, so that the material flow can simultaneously fill each cavity.

8. Low mold temperature

Low mold temperature can accelerate the solidification process of plastic, thereby reducing its fluidity. When the mold temperature is too low, the flow of plastic melt in the mold cavity will be restricted, resulting in insufficient filling. To solve this problem, it is necessary to increase the mold temperature to slow down the solidification rate of the plastic and improve its fluidity.

9. Insufficient injection pressure and speed

Injection pressure and speed are important factors affecting the filling effect. When the injection pressure is insufficient, the pressure of the plastic melt in the mold cavity is not enough to overcome the flow resistance; When the injection speed is insufficient, the flow time of the plastic melt in the mold cavity will be prolonged, thereby increasing the risk of solidification. To solve this problem, it is necessary to increase the injection pressure and speed to ensure that the plastic melt can smoothly fill the entire mold cavity.

10. The injection stroke is too short

A short injection stroke can lead to insufficient supply, as there is not enough space for the plastic melt to fill the entire mold cavity during the injection process. To solve this problem, it is necessary to adjust the length of the injection stroke and check the feeding port of the particle bridging or adjust the nozzle backflow valve to ensure sufficient feeding volume.