Injection molding production of main products are:
Children's toys, electronic products, daily necessities, medical supplies, auto parts, building components etc., generally used raw materialS: ABS, HIPS, PC/ABS, PP, PVC, PMMA, PC, POM, etc.
Plastic raw materials can be divided into: thermoplastic and thermosetting plastic.
Engineering plastics:
General engineering materials: PA(PA6\66\1010\11\12), PC, POM, PBT, PET, PPO, PMMA,
Special engineering materials: PPS LCP PI PTFE PES PEI PKKE PAI PAR,
Plastic alloy: PPO/PS PC/ABS PC/PBT PC/PET PA/PP, etc
For example: Computer case shell used raw materials are generally these kinds: ABS,HIPS,PC/ABS and so on. Audio or remote control may add fiber raw material!