1, Steel materials
Steel materials are one of the most commonly used mold materials in permanent casting, with high hardness, good heat resistance, and high strength, which can meet the needs of most casting processes.
Cold work mold steel: It has good wear resistance and toughness, and is suitable for manufacturing molds with complex shapes and high precision requirements. Materials such as Cr12MoV and Cr12, after heat treatment, have a hardness of over 60HRC and significantly improved wear resistance, but their toughness has decreased. Therefore, it is necessary to control the heat treatment process reasonably.
Hot work die steel: mainly used for manufacturing molds that work at high temperatures, such as die-casting molds, hot forging dies, etc. This type of material has good thermal stability and thermal fatigue resistance, such as 5CrNiMo, 5CrMnMo, etc., which can maintain high hardness and strength at high temperatures, reducing thermal deformation and cracking of molds.
Hard alloy steel: It is a high-performance mold material with characteristics such as high hardness, high strength, high wear resistance, and high corrosion resistance. Suitable for manufacturing high-precision, high load molds, such as precision stamping dies, deep drawing dies, etc. However, hard alloy steel is expensive and difficult to process, requiring strict control of processing and heat treatment processes.
2, Cast iron material
Cast iron materials play an important role in permanent mold casting due to their excellent wear resistance, corrosion resistance, and high temperature resistance.
Gray cast iron: It has good casting and mechanical properties, low cost, and is suitable for manufacturing large and structurally simple molds. However, the hardness and strength of gray cast iron are relatively low, making it unsuitable for high-precision and high load molds.
Ductile iron: Through spheroidization treatment, the graphite in cast iron is distributed in a spherical shape, significantly improving the strength and toughness of cast iron. Ductile iron molds have high hardness and wear resistance, making them suitable for manufacturing molds with medium load and medium precision, such as die-casting molds, injection molds, etc.
Creep graphite cast iron: The graphite morphology of creep graphite cast iron is between gray cast iron and ductile iron, and it has excellent strength, toughness, and wear resistance. Creep graphite cast iron molds are suitable for manufacturing high-precision, high load molds, such as engine cylinder blocks, cylinder heads, etc.
3, Aluminum alloy material
Aluminum alloy molds have been widely used in the manufacturing of small and complex components due to their advantages of light weight, high dimensional accuracy, and good processing performance.
Casting aluminum alloys such as A356, A380, etc. have good casting and mechanical properties, suitable for manufacturing small and structurally complex molds. However, the hardness and wear resistance of aluminum alloys are relatively low, and their wear resistance needs to be improved through heat treatment or surface treatment techniques.
Forged aluminum alloys, such as 2024, 7075, etc., have high strength and hardness, and are suitable for manufacturing molds with medium load and medium precision. However, the cost of forging aluminum alloy is high and the processing difficulty is high, requiring strict control of the processing and heat treatment processes.
4, Other materials
In addition to the common mold materials mentioned above, there are also some special materials that have been applied in permanent mold casting.
Zinc based alloys, such as ZA12, ZA27, etc., have good strength and hardness while maintaining a certain degree of ductility. Zinc based alloy molds are suitable for manufacturing mechanical parts that can withstand high loads, such as bearings, gears, etc. However, the corrosion resistance of zinc based alloys is poor and needs to be improved through surface treatment.
Ceramic materials: have high hardness, high wear resistance, high corrosion resistance, and high temperature resistance. Ceramic molds are suitable for manufacturing molds used under high temperature and high pressure, such as ceramic injection molds, ceramic die-casting molds, etc. However, the brittleness, processing difficulty, and high cost of ceramic materials limit their widespread application.
Nov 01, 2024
Leave a message
What are some common mold materials for permanent mold casting?
Send Inquiry