Raw materials for rubber molds

At the rubber mold factory, one of our most important processes is the rubber mold process, which is the core technology of the rubber mold factory

Let's talk about the silicone rubber raw material in the common rubber mold factory

Mold silicone rubber is generally composed of base rubber, cross-linking agent, catalyst, filler, etc.

The base glue is 107 silicone rubber, called hydroxyl terminated polydimethylsiloxane.

This mold silicone rubber can be cured at room temperature, has good fluidity, no deformation, and only a slight linear shrinkage.

The cross-linking agent is ethyl orthosilicate. The amount of cross-linking agent has a significant effect on the curing time, tear strength and elongation of silicone rubber. Practice has shown that the amount of cross-linking agent should be 5% (mass fraction) of the base rubber.

The catalyst is dibutyltin dilaurate. The amount of catalyst added has a direct relationship with the curing time, it should not be too much, generally 1% ~ 2% (mass fraction).

Fillers include talc powder, quartz powder, and white carbon black. Talc powder is generally used as filler. If white carbon black is used as filler, the mechanical strength, tear strength and uniformity are significantly improved.