1, Injection molding
Injection molding is a kind of molding process by injecting melted plastic into the mold, making it cool and solidify in the mold, and finally obtaining the desired product. Injection molding machine is the main equipment of injection molding, through high-pressure injection of plastic, make it fill the entire mold cavity. Common injection molding machines include vertical injection molding machines and horizontal injection molding machines, and their choice depends on the size and shape of the product.
Characteristics of injection molding:
High precision: injection molding can realize high-precision manufacturing of complex parts, which is suitable for fields with high requirements for product size and shape.
High production efficiency: the cycle time of injection molding is relatively short, which is suitable for mass production.
Good surface quality: the surface quality of the product is good because the plastic is fully filled in the mold cavity while being injected under high pressure.
Process flow of injection molding:
Plastic granule feeding
Heating and melting of plastics
High pressure injection
Cooling solidification
Open the mold and take out the finished product
2, Molding
Molding is a process in which plastic particles are heated to a molten state, placed in a mold, and shaped by applying a certain amount of pressure. Compared with injection molding, molding has less requirements for the melting process of plastics, and is suitable for some heat sensitive plastics.
Characteristics of molding:
Wide range of application: molding is suitable for all kinds of plastics, including materials with strong thermal sensitivity.
Low cost: the molding equipment is relatively simple and the cost is relatively low, which is suitable for small batch production.
Suitable for large-scale products: molding is suitable for manufacturing some large-scale products, such as large shells, plates, etc.
Process flow of molding:
Plastic particles are heated and melted
Put the melted plastic into the mold
Apply certain pressure
Cooling solidification
Open the mold and take out the finished product
3, Difference and comparison between injection molding and molding
Principle difference:
Injection molding fills the mold cavity with melted plastic through high-pressure injection, while molding is to place plastic in the mold and apply pressure for molding at a certain temperature.
Scope of application:
Injection molding is suitable for areas that require high product accuracy and surface quality and require mass production. And molding is suitable for all kinds of plastics, especially some materials with strong thermal sensitivity, suitable for small batch production and large-scale product manufacturing.
Productivity and cost:
Injection molding is suitable for large-scale production and has high production efficiency. Relatively speaking, the molding equipment is simple and the cost is low, which is suitable for small-scale and medium and small batch production.
Product size and shape:
Injection molding is suitable for producing small and complex products, while molding is suitable for larger products, such as large plates, shells, etc.