Camera Lens Injection Molded Parts
Custom injection molded parts for Optical Camera Lens
A camera lens (also known as photographic lens or photographic objective) is an optical lens or assembly of lenses used in conjunction with a camera body and mechanism to make images of objects either on photographic film or on other media capable of storing an image chemically or electronically.
Powerfulsky Mould supplied high grade injection molding plastic parts for customized camera lens.
Products Information | ||
Product Description | Part Name | Camera lens injection molded parts |
Part Material | ABS | |
Part Size(MM) | 120*55*54 | |
Mould Steel | A plate | S50C |
B plate | S50C | |
Cavity Insert | S136 (HRC 45-50 ) | |
Core Insert | S136 (HRC 45-50 ) | |
Slider Insert | 2344 | |
Ejector Plate | S50C | |
Spare Parts | S50C | |
Mould Description | Mould Size(L*W*H MM) | 1000*780*600 |
Mould Gross Weight(KGS) | 2965 | |
Mould Life Time(Shots) | 1,000,000 | |
Mould Manufacturing Cycle | 25 days | |
Surface Finish | Polishing | |
Runner Description | Cold runner | |
Ejection System | Eject blade | |
Cycle Time(Second) | 25s | |
Injection Gate Type | Side gate | |
Hot Tags: camera lens injection molded parts, China, manufacturers, suppliers, factory, customized, made in China, Pulse Oximeter In Stock, Blue Bireless Speakers Mold, Pulse Oximeter Mold, Toys Products Injection Mold, OpenTop Indoor Bin Hotel Room Bins, PP Large Size Waste Trash Can Injection Mold